A Traditional, NON CORROSIVE Longrifle Hardware Finish | Kibler Kit Class NMLRA | Fire Bluing Finish

Описание к видео A Traditional, NON CORROSIVE Longrifle Hardware Finish | Kibler Kit Class NMLRA | Fire Bluing Finish

➽ ➽ Support the channel - nmlra.org/join ➽ ➽
Step into the classroom as Mike Brooks and Wayne Estes teach students how to assemble their own Kibler Longrifle Kits.

In this video, we follow along as Wayne Estes shows a student how to fire blue the metal hardware for their Kibler Southern Mountain Rifle Muzzleloader kit

While the torch and oil used was not available to the American muzzleloader builders of the 18th and 19th centuries, the finish we achieve in this video is similar to those that could have been used by builders generations ago.

Find out more about these classes at NMLRA.org/education
0:00 Fire Bluing Basics
0:33 Trigger Guard Fire Bluing
1:33 Why this is a great finish for locks and triggers
2:17 The Final Look


➽ ➽ Muzzle Loading & Living History Books, Merch, and More - nmlra.org/store

Click here to SUBSCRIBE - http://bit.ly/NMLRAYT

The NMLRA exists to promote, support, nurture, and preserve our nation’s rich historical heritage in the sport of muzzleloading through recreational, educational, and historical venues.

Since 1933, we have led the effort to preserve the history of the United States through muzzleloading shooting sports & living history events.

Website: NMLRA.org
Podcast: NMLRA.org/podcast
Instagram: Instagram.com/muzzleblasts
Facebook: facebook.com/NMLRA
Facebook Group: facebook.com/groups/NMLRA